      Properties of La(Fe, Si)13 Magnetocaloric compounds prepared by reactive spark plasma sintering.

      data
      PAUL-BONCOUR V., PATISSIER A., NAKOURI K., et al.
      International Institute of Refrigeration (IIR)
      LANTHANUM, IRON, SILICON, ALLOY, MAGNETIC PROPERTY, MEASUREMENT

      Read this article at

      ScienceOpenPublisher
      Bookmark
          There is no author summary for this article yet. Authors can add summaries to their articles on ScienceOpen to make them more accessible to a non-specialist audience.

          Abstract

          La(Fe, Si)13 magnetocaloric compounds have been synthesized by high energy ball milling (BM) and sintered by Spark Plasma Sintering (SPS), starting either from an already annealed sample or from a non-annealed sample (reactive sintering). It is possible to form the NaZn13 phase directly by reactive sintering at only 1273K. The influence of the annealing temperature has been investigated in details as well as other parameters. The properties of sintered compounds have been compared with those of samples which were only prepared by BM and annealed.

          Related collections

          Author and article information

          Journal
          International Institute of Refrigeration (IIR)
          2016
          Article
          10.18462/iir.thermag.2016.0075
          96139c8e-ae2b-41f9-9f81-7bd75caa1853
          History

          SILICON,MAGNETIC PROPERTY,IRON,ALLOY,LANTHANUM,MEASUREMENT
          SILICON, MAGNETIC PROPERTY, IRON, ALLOY, LANTHANUM, MEASUREMENT

          Comments

          Comment on this article