      Structural Control on Clay Mineral Authigenesis in Faulted Arkosic Sandstone of the Rio do Peixe Basin, Brazil

      , , , , , , ,
      Minerals
      MDPI AG

      Read this article at

      Bookmark
          There is no author summary for this article yet. Authors can add summaries to their articles on ScienceOpen to make them more accessible to a non-specialist audience.

          Abstract

          Clay minerals in structurally complex settings influence fault zone behavior and characteristics such as permeability and frictional properties. This work aims to understand the role of fault zones on clay authigenesis in arkosic, high-porosity sandstones of the Cretaceous Rio do Peixe basin, northeast Brazil. We integrated field, petrographic and scanning electron microscopy (SEM) observations with X-ray diffraction data (bulk and clay-size fractions). Fault zones in the field are characterized by low-porosity deformation bands, typical secondary structures developed in high-porosity sandstones. Laboratory results indicate that in the host rock far from faults, smectite, illite and subordinately kaolinite, are present within the pores of the Rio do Peixe sandstones. Such clay minerals formed after sediment deposition, most likely during shallow diagenetic processes (feldspar dissolution) associated with meteoric water circulation. Surprisingly, within fault zones the same clay minerals are absent or are present in amounts which are significantly lower than those in the undeformed sandstone. This occurs because fault activity obliterates porosity and reduces permeability by cataclasis, thus: (1) destroying the space in which clay minerals can form; and (2) providing a generally impermeable tight fabric in which external meteoric fluid flow is inhibited. We conclude that the development of fault zones in high-porosity arkosic sandstones, contrary to other low-porosity lithologies, inhibits clay mineral authigenesis.

          Related collections

          Most cited references30

          • Record: found
          • Abstract: not found
          • Article: not found

          A review of recent developments concerning the structure, mechanics and fluid flow properties of fault zones

            Bookmark
            • Record: found
            • Abstract: not found
            • Article: not found

            Clay gouge

              Bookmark
              • Record: found
              • Abstract: not found
              • Article: not found

              Deformation bands in sandstone: a review

                Bookmark

                Author and article information

                Journal
                MBSIBI
                Minerals
                Minerals
                MDPI AG
                2075-163X
                September 2018
                September 14 2018
                : 8
                : 9
                : 408
                Article
                10.3390/min8090408
                e1ee7cdd-8658-43da-bb45-c7a5e7dc7e54
                © 2018

                https://creativecommons.org/licenses/by/4.0/

                History

                Comments

                Comment on this article